Adding glass fibers to nylon dramatically changes its performance characteristics. While unfilled nylon offers excellent toughness and processability, glass-filled grades deliver substantially higher strength, stiffness, and thermal stability.
What Is Glass-Filled Nylon?
Glass-filled nylon is a composite material consisting of nylon resin reinforced with short glass fibers. The most common grades contain 15%, 25%, 30%, or 50% glass fiber by weight.
기계적 특성 비교
| 속성 | PA6 Unfilled | PA6 GF15 | PA6 GF30 | PA6 GF50 |
|---|---|---|---|---|
| 인장 강도(MPa) | 75 | 120 | 170 | 210 |
| 굴곡 탄성률(GPa) | 2.7 | 5.5 | 8.5 | 14.0 |
| 1.8 MPa에서의 HDT (°C) | 65 | 180 | 195 | 210 |

치수 안정성
Glass fibers reduce the material’s coefficient of linear thermal expansion (CLTE) by 50-70%, bringing it closer to metals like aluminum.

처리 고려 사항
Glass-filled nylon requires: higher melt temperatures, higher injection pressures, hardened molds due to abrasive wear, and careful gate design for fiber orientation.

Cost Considerations
GF30 provides the best balance of cost and performance for most applications. It’s the most widely used glass-filled grade.
Application Guide
Choose Unfilled Nylon When:
- Impact resistance and toughness are critical
- Parts need good surface finish
- Snap-fits or living hinges are required
- Cost is the primary concern
Choose Glass-Filled Nylon When:
- High strength and stiffness are needed
- Dimensional stability under heat is critical
- Metal replacement is the goal
- Precision tolerances must be maintained
Our Capabilities
With over 300 CNC machines, we produce more than 10,000 pieces daily with tolerances as tight as ±0.005mm. We accept MOQ from 1 piece, with delivery times ranging from 24 hours to 15 days. We supply nylon in all grades—unfilled, GF15, GF30, and GF50. Get a quote within 24 hours.
자주 묻는 질문
How do you know whether Glass-Filled vs Unfilled Nylon: Complete Performance Comparison fits a part?
Glass-Filled vs Unfilled Nylon: Complete Performance Comparison fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.
What properties should be checked for Glass-Filled vs Unfilled Nylon: Complete Performance Comparison?
강도, 강성, 내충격성, 내열성, 수분 흡수율, 치수 안정성, 마찰, 마모 및 화학적 호환성을 확인하십시오.
What is the biggest selection risk for Glass-Filled vs Unfilled Nylon: Complete Performance Comparison?
가장 큰 위험은 실제 환경, 가공 방법, 부품 형상 및 장기 사용 등을 고려하지 않고 데이터시트에 기재된 수치만 보고 선택하는 것입니다.
When should Glass-Filled vs Unfilled Nylon: Complete Performance Comparison be tested before production?
부품이 하중, 열, 화학 물질, 습기, 엄격한 공차, 규제 요건 또는 새로운 작동 환경에 노출될 경우 시험을 실시하는 것이 좋습니다.