Why Lubricate Nylon?
Nylon’s natural surface properties include a relatively low coefficient of friction compared to many engineering plastics—but it’s not inherently self-lubricating. In moving-part applications like gears, bearings, slides, and cams, unlubricated nylon can experience accelerated wear, frictional heating, and stick-slip behavior. Lubricated nylon grades solve this by incorporating solid or liquid lubricants directly into the polymer matrix, creating parts that run smoothly for millions of cycles without external lubrication.
The lubricant additives work by forming a transfer film on the mating surface. As the nylon part moves, microscopic lubricant particles are released, coating both the nylon surface and the opposing metal or plastic surface. This film reduces the coefficient of friction from 0.35–0.40 (unmodified nylon on steel) down to 0.10–0.20, depending on the lubricant type and loading.
The Three Main Lubricant Types
| Lubricant | Typical Loading | COF (vs Steel) | 최고의 애플리케이션 |
|---|---|---|---|
| PTFE(테프론) | 10–20% | 0.10–0.18 | High-speed bearings, low-load slides |
| MoS₂ (Molybdenum Disulfide) | 1–5% | 0.12–0.20 | High-load gears, thrust washers |
| Oil-filled | 2–8% | 0.08–0.15 | Precision bearings, low-noise applications |
PTFE-Filled Nylon
PTFE (polytetrafluoroethylene) is the most common solid lubricant for nylon. With a coefficient of friction as low as 0.04 in its pure form, PTFE particles dispersed throughout nylon create an extremely low-friction surface. PTFE-filled nylons are ideal for high-speed, low-to-moderate load applications where continuous sliding motion is required.
The limitation: PTFE reduces mechanical strength by 10–20% and increases cost. It also doesn’t perform as well as MoS₂ under very high contact pressures.
MoS₂-Filled Nylon
Molybdenum disulfide has a layered crystal structure similar to graphite—sheets that easily slide past each other. This makes it exceptional under high contact pressures where PTFE would be squeezed out. MoS₂-filled nylon is the go-to choice for gears, cams, and thrust washers operating under significant load.
MoS₂ also increases nylon’s crystallinity slightly, which can improve strength and stiffness—unlike PTFE which weakens the matrix. The dark gray/black color can be a consideration for visible parts.
Oil-Filled Nylon
Oil-filled nylons incorporate lubricating oil directly into the polymer during compounding. During operation, the oil slowly migrates to the surface, providing continuous lubrication throughout the part’s life. This “self-replenishing” characteristic makes oil-filled nylon excellent for sealed applications where relubrication is impossible.
Common oils include silicone, mineral oil, and synthetic hydrocarbon oils. The oil content is precisely controlled to avoid excessive migration that could contaminate surrounding components.


Wear Rate Comparison
| 나일론 등급 | K-Factor (×10⁻⁸ mm³/N·m) | PV Limit (MPa·m/s) | Service Temp Range |
|---|---|---|---|
| PA6 (충진제 미첨가) | 40–80 | 0.09–0.12 | -30°C to 85°C |
| PA6 + 15% PTFE | 5–12 | 0.15–0.25 | -40°C to 100°C |
| PA6 + MoS₂ | 8–15 | 0.20–0.35 | -30°C to 95°C |
| PA66 + Aramid + PTFE | 2–5 | 0.35–0.50 | -40°C to 120°C |
Design Guidelines for Lubricated Nylon Parts
- Surface finish of the mating part: Aim for 0.2–0.4 μm Ra on the steel/opposing surface. Rougher surfaces accelerate wear.
- Clearance: Allow 0.3–0.5% of the bearing diameter for thermal expansion and water absorption swell.
- Wall thickness: Maintain uniform wall thickness to avoid warpage that creates uneven wear patterns.
- Running-in period: Expect higher friction during the first 500–1000 cycles as the transfer film establishes.
- Combination with glass fiber: Adding glass fiber to lubricated nylon improves load capacity but increases wear on the mating surface. Use hardened steel (58+ HRC) for mating parts.
엔지니어링 플라스틱에 나일론 플라스틱을 선택해야 하는 이유는?
- ✅ 300대 이상의 사출 성형기 50T에서 2000T까지
- ✅ 하루 10,000개 이상의 부품 생산 능력
- ✅ ±0.02mm 정밀도 모든 재료에 대한 허용 오차
- ✅ MOQ 단 1개 프로토타이핑용, 수백만 개로 확장 가능
- ✅ 24시간 견적, 리드 타임 3~15일
- ✅ ISO 9001 인증 품질 관리 시스템
자주 묻는 질문
How do you know whether Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications fits a part?
Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.
What properties should be checked for Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications?
강도, 강성, 내충격성, 내열성, 수분 흡수율, 치수 안정성, 마찰, 마모 및 화학적 호환성을 확인하십시오.
What is the biggest selection risk for Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications?
가장 큰 위험은 실제 환경, 가공 방법, 부품 형상 및 장기 사용 등을 고려하지 않고 데이터시트에 기재된 수치만 보고 선택하는 것입니다.
When should Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications be tested before production?
부품이 하중, 열, 화학 물질, 습기, 엄격한 공차, 규제 요건 또는 새로운 작동 환경에 노출될 경우 시험을 실시하는 것이 좋습니다.
What should a lubricated nylon grade review include for a wear component?
Identify the mating material, surface condition, load, speed, duty cycle, temperature and whether external lubrication is permitted. Specify critical dimensions and moisture or chemical exposure. Compare the actual PTFE, MoS2 or oil-modified grade with the same wear test or part validation; an additive label alone does not establish friction or service life for the application.